Home > News > Daily News > Aluminum die casting defects and prevention
News
Daily News
Industry News
Company news
Certifications
Latest News

Gifts of love in ancient China

Jade pendants The ancient Chinese usually gave their lovers something small so that they could easily take it everywhere. A jade pendant is a good cho...

what is mild steel

Mild steel is a type of carbon steel with a low amount of carbon – it is actually also known as “low carbon steel.” Although ranges vary depending ...

What is ALOCROM 1200 surface treatment

What is ALOCROM 1200surface treatment Alocrom 1200 is a rapidnon-electrolytic dip process which gives excellent protection against corrosionto both pa...

What is Kydex material

What is Kydexmaterial Kydex is a line of thermoplasticacrylic-polyvinyl chloride materials manufactured by Sekisui SPI. It has a widevariety of applic...

10 Differences between a Businessman and Entrepreneur

10 Differences between a Businessman and Entrepreneur Business people and entrepreneurs have many similarities.However, they are not the same kind of ...

Aluminum alloy die-casting heat treatment technology

Aluminum alloy die casting skills is to choose a standard heat treatment, heat treatment to control the heating rate rises to a corresponding temperature cooling

What is Over mold?

Overmolding is also called 2 times injection molding in China. Compared with the third-party material bonding, overmolding process makes the process f...

How and When to Add Bend Reliefs to Sheet Metal Parts

What is a Bend Relief? A bend relief is nothing more than two small incisions cut into a piece of sheet metal to free the metal between the two. It se...

What is Black Oxide?

Black Oxide, blackening, oxidizing, oxiding, black passivating, gun bluing . . . these terms all refer to the process of forming a black iron oxide on...

What is Alodine 5200 surface treatment

What is Alodine 5200surface treatment Alodine 5200 treatment is a chromiumfree product and specifically formulated for treating aluminium and its allo...
Contact Us
Sales Manager: Edith
Tel:86 151 1311 0489
Tel:86 755 8273 7469
E-mail: sales820@xy-global.com
Postal Code: 518129
Office Address: Room1702,17F, Building 4,Tian'an Cloud Park, No. 2018 Xuegang Rd., Longgang District, Shenzhen, China
Factory Address: Daling Industrial Area, Shaling, Fenggang Town, Dongguan City, Guang Dong, China Contact Now

Aluminum die casting defects and prevention

Aluminum die casting defects and prevention

kerry 2021-12-02 20:52:50

one. Adhesive traces
Appearance inspection: small flakes and metal or non-metallic and metal base parts are welded, and the small flakes are peeled off under the action of external force. After the peeling, the surface of the casting is bright and some are dark gray.

  The reasons are as follows:
 
  (1) There are metallic or non-metallic residues on the surface of the die-casting cavity;
(2) When pouring, the impurities are first brought in and attached to the surface of the cavity.
 
The solutions and prevention methods are:
 
  (1) Before die-casting, the cavity pressure chamber and gating system should be cleaned up to remove metal or non-metal adherents;
  (2) Clean up the cast alloy;
  (3) Choose a suitable paint, and the coating should be even.
 
two. Layering (skinning and peeling)
 
  Visual inspection or damage inspection: There are obvious layers of metal in the casting part.
 
  The reasons are as follows:
 
  (1) The mold is not rigid enough. During the molten metal filling process, the template shakes;
  (2) The punch appears to crawl during the injection process;
  (3) Improper design of runner system.
   The solutions and prevention methods are:
 
(1) Strengthen the rigidity of the mold and tighten the mold parts to make them stable;
(2) Adjust the cooperation of the injection punch and the pressure chamber to eliminate the crawling phenomenon;
(3) Reasonably design the inner runner.


 
three. Friction ablation
Visual inspection: The surface of the die-casting part has rough surfaces in some positions.
The reasons are as follows:
 
(1) Improper position, direction and shape of the inner runner caused by the die-casting mold (mold);
(2) Insufficient cooling of the parts where molten metal is scoured severely at the inner runner caused by the casting conditions.
 
The solutions and prevention methods are:
 
(1) Improving the location and direction of the inner runner where it is not good at pouring;
(2) Improve the cooling conditions, especially the areas where the molten metal is violently scoured;
(3) Add paint to the ablated part;
(4) Adjust the flow rate of the alloy liquid to prevent cavitation
(5) Eliminate the alloy adherents on the mold (mold).
 
Four. Erosion
 
  Visual inspection: There are pitting or embossing in the local position of the die casting.
 
  The reasons are as follows:
 
  (1) Improper location of the inner runner;
 
  (2) Poor cooling conditions.
 
  The solutions and prevention methods are:
 
  (1) The thickness of the inner runner should be appropriate;
 
  (2) Modify the position, direction and setting method of the inner runner;
 
  (3) Strengthen the cooling of the eroded parts.
 
five. Crack
 
  Visual inspection: Put the casting in alkaline solution, the cracks are dark gray. The destruction and cracking of the metal matrix is ​​straight or wavy, with narrow and long lines, which tend to develop under the action of external forces.